阳光板安装方法产品特性(其他屋顶和覆盖材料不具备)1、抗紫外线辐射抗老化利用空挤压工艺在耐候性脆弱的PC板材上空挤压UV树脂,板面均匀分布有高浓度的UV层,阻挡紫外线的穿过,防止板材黄变,延长板材寿命使产品使用寿命达到10年以上。
并且产品具有长期持续透明性的特点。
2、强隔热保温性能PC阳光板的中空结构,其隔热性能大大优于其它实心材料,是农业温室及其它隔热装置的首选材料。
阳光板还具有很好的隔音性能,是高速公路等的首选材料。
、难燃性 3PC阳光板具良好防火性,为难燃B1级,自燃温度为630?,发生燃烧时不会助长火势蔓延,也不会产生浓烟及有毒气体,离火自熄,具良好阻燃防火性能。
4、质轻环保、不易折断10mm厚的板材比6mm厚的钢化玻璃轻85%,对施工即轻便又结实。
5、可冷弯质轻且可以直接冷弯,施工简便且加工良好。
6、抗冲击性板材在-40?至+120?之间,并长期暴露于室外,都具有优良的抗冲击性能,最重要的是在这样的条件下,板材不破碎。
7、透光性好透明PC板透光率高达88%,透明阳光板的透光率高达80%,透明度不会因使用时间而降低,着色阳光板能阻挡太阳光线中最强的部分,使透过的光线柔和。
8、形稳性板材长期在复杂极端的温度条件下,仍然保持良好的抗冲击性和刚性。
安装方法常用安装方法手电钻、玻璃胶枪accident responsibility, give notice of criticism and 50-100economic sanctions against them. (4) to conceal the accident, reported without undue delay or false, to inform the administrative leadership of the criticism, resulting in serious consequences, the pursuit of leadership, along with 500-1000 punishment. (5) significant near miss should be attempted as the case of responsible for the accident and construction team injuries accident penalty provisions, mutatis mutandis. Eight, should perform in the construction standards and specifications, serial number a 1 GB3323-2005 steel fusion welded butt joints, welding engineering-Ray lighting and quality rating of 2 GB11345-89 steel welds manual methods of ultrasonic inspection and testing results for grade 3 GB50236-2002 industrial pipe welding engineering code for construction and acceptance of field equipment 4 HGJ222-92 technical specificationfor welding of aluminium and its alloys 5 low temperature steel welding procedure 6 SH3525-2004 petrochemical JB/ T4708-2000 of welding procedure qualification for steel pressure vessels 7 JB/4709-2000 8JB4730-2005 pressure vessel welding procedures of steel pressure vessel NDT 9 JB/T4744-2000 steel pressure vessel products mechanical properties test of welded plate II, mechanical equipment installation engineering 1 GB150-98 2 GB50128-2005 vertical cylindrical steel pressure vessel steelwelded specification for construction and acceptance of oil tank 3 JB/ T4735-1997 steel一、嵌入式安装法a 保护膜会影响填缝料与中空板的结合,故在嵌入安装前,请先去掉嵌入量为5-10cm宽的保护膜。
b 板材热胀冷缩系数与支撑框架不同,且需要留余量以承受风压、雪压等,因此嵌入量要预留充分,以及热胀冷缩的空间。
一般板材边缘伸入固定框架25mm以上,并至少有二条筋肋安装进固定区域;热胀冷缩一般每米留3mm空隙。
(热膨胀率为 0.065mm/moC) 二、螺丝安装法a、螺栓或铆钉穿孔安装时,板材的开孔孔径须比螺栓或铆灯直径大50,,预留热胀冷缩空间。
b、所有孔穴均应以硅酮密封胶填满空隙及覆盖外露部分,防止水分或清洁济进入,影响板材质量。
c、铆钉头部应比柄部大2倍,并加上垫片,避免在局部产生大压强损坏板材。
d、螺丝不宜拧得太紧,避免压裂板材。
e、不宜使用PVC垫片或含沥青成份的防水胶布。
f、冷弯加工时,弯曲部分避免使用螺丝固定。
accident responsibility, give notice of criticism and 50-100 economic sanctions against them. (4) to conceal the accident, reportedwithout undue delay or false, to inform the administrative leadership of the criticism, resulting in serious consequences, the pursuit of leadership, along with 500-1000 punishment. (5) significant near miss should be attempted as the case of responsible for the accident and construction team injuries accident penalty provisions, mutatis mutandis. Eight, should perform in the construction standards and specifications, serial number a 1 GB3323-2005 steel fusion welded butt joints, welding engineering-Ray lighting and quality rating of 2 GB11345-89 steel welds manual methods of ultrasonic inspection and testing results for grade 3 GB50236-2002 industrial pipe welding engineering code for construction and acceptance of field equipment 4 HGJ222-92 technical specificationfor welding of aluminium and its alloys 5 low temperature steel welding procedure 6 SH3525-2004 petrochemical JB/ T4708-2000 of welding procedure qualification for steel pressure vessels 7 JB/4709-2000 8JB4730-2005 pressure vessel welding procedures of steel pressure vessel NDT 9 JB/T4744-2000 steel pressure vessel products mechanical properties test of welded plate II, mechanical equipment installation engineering 1 GB150-98 2 GB50128-2005 vertical cylindrical steel pressure vessel steel welded specification for construction and acceptance of oil tank 3 JB/T4735-1997 steel三、PC板材曲板安装越美板材可以按照弯曲构型进行弯曲安装,但板材弯曲半径不可以小于其最小弯曲半径,这样因弯曲而引入的应力就不会影响板材的机械性能。
板材一定要顺着长度方向安装,不能沿着宽度方向安装。
不仅提高采光面积,符合建筑艺术设计弯曲要求。
而且提高了板材的承载能力,普通玻璃是望尘莫及的。
板材允许弯曲的正确方向,见下图accident responsibility, give notice of criticism and 50-100economic sanctions against them. (4) to conceal the accident, reported without undue delay or false, to inform the administrative leadership of the criticism, resulting in serious consequences, the pursuit of leadership, along with 500-1000 punishment. (5) significant near miss should be attempted as the case of responsible for the accident and construction team injuries accident penalty provisions, mutatis mutandis. Eight, should perform in the construction standards and specifications, serial number a 1 GB3323-2005 steel fusion welded butt joints, welding engineering-Ray lighting and quality rating of 2 GB11345-89 steel welds manual methods of ultrasonic inspection and testing results for grade 3 GB50236-2002 industrial pipe welding engineering code for construction and acceptance of field equipment 4 HGJ222-92 technical specificationfor welding of aluminium and its alloys 5 low temperature steel welding procedure 6 SH3525-2004 petrochemical JB/ T4708-2000 of welding procedure qualification for steel pressure vessels 7 JB/4709-2000 8JB4730-2005 pressure vessel welding procedures of steel pressure vessel NDT 9 JB/T4744-2000 steel pressure vessel products mechanical properties test of welded plate II, mechanical equipment installation engineering 1 GB150-98 2 GB50128-2005 vertical cylindrical steel pressure vessel steel welded specification for construction and acceptance of oil tank 3 JB/T4735-1997 steelPC板的安装说明1、安装前必须保证骨架的平整和清洁;2、先检查板材的裁切尺寸和膨胀预留量是否合格,要特别注意留出足够的均匀的膨胀间隙,计算公式如下:总膨胀间隙,膨胀系数×当地安装前后最大的温差×板材长度-5 线性热膨胀系数为7.0×10mm/mm.K,即温度每升高1度,1m×1m的板材顺着长宽方向-5各膨胀7.0×10mm(0.07mm)3、板材热胀冷缩系数与支撑框架不同,且需要留余量以承受风压、雪压等,因此嵌入量要预留充分,以及热胀冷缩的空间。