Location:pWPS No.:
焊接方法:t101 坡口准备和清理:机械加工、化学清洗Welding process:t101 preparation and cleaning:Machining,chemical clean 接头类型:BW 焊接设备:肯倍FastMig Pulse 350 Joint type:BW W elding Equipment: KEMPPI FastMig Pulse 350 焊接位置:PA 焊工姓名:
Welding positions:PA Welder,s name:
母材规格(mm):300*300*3 钨极种类/直径(mm):
Parent metal size(mm):300*300*3 Tungsten electrode type/size:
母材质保书:GB5237 6063T5 焊材烘干规定:
Base metal specification:GB5237 6063T5 Special baking or drying:
焊材质保书:ER5356 53M010512 清根情况:
Filler material specification:ER5356 53M010512 Back gouping:
焊接工艺参数【Welding details】:
Preheat temperature:Other information:
层间温度(℃):基值电流/峰值电压:
Interpass temperature:Base current/Peak voltage:
钨极种类/直径(mm):脉冲频率:
Tungsten electrode type/size:Pulse frequency:
干伸长度(㎜):12 脉冲时间:
D i s t a n c e c o n t a c t t u b e/w o r k p i e c e:12 Pulse time:
焊枪角度(°):弧长/微调:
Torch angle : Arc length/Fine adjust:
焊后热处理:摆动(焊道的最大宽度)(㎜):
Post-weld heat treatment:W e a v i n g(M a x i m u m w i d t h o f r u n):
时间、温度、方法:振动(振幅、频率、停留时间):
T im e、tem perature、m ethod:O s c i l l a t i o n(Am p l i t u d e,f r e q u e n cy,d w e l l t i m e):
加热和冷却速度(℃/h):等离子焊接细节:
Heating and cooling rates:Torch angle:
制造商:
Manufacture:。